Customization: | Available |
---|---|
Material: | Organic Silicone |
Application: | Industrial |
Still deciding? Get samples of US$ 5/kg
Order Sample
|
Shipping Cost: | Contact the supplier about freight and estimated delivery time. |
---|
Payment Methods: |
|
---|---|
Support payments in USD |
Secure payments: | Every payment you make at Made-in-china.com is protected by the platform. |
---|
Refund policy: | Claim a refund if your order doesn't ship, is missing, or arrives with product issues. |
---|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
High tear tin liquid silicone rubber for epoxy resin casting
Product description of tin silicone rubber
Tin cure silicone rubber are two compounds, liquid, tin cured silicone rubber that have exceptional tear strength and working properties, cured in room temperature. A range of materials can be casted into the cured silicone molds : plaster, gypsum, concrete , wax, polyurethane ,polyester resin .
Applications of tin cure silicone rubber
1.Art and decoration: soap, candle, aquarium decoration, crafts molds.
2.Furniture: concrete ,GFRC furniture, artificial stone molds
3.Architecture: column, fountain molds, architectural restoration
1 .Outstanding release properties
2. High flowability and long working time
3. High tear strength & tear strength
4. High elasticity, for easy removal of complex replica parts
5. Can add thixotropic for vertical surface application
Model Code | GTSIL-T05 | GTSIL-T10 | GTSIL-T15 | GTSIL-T20 | GTSIL-T25 | GTSIL-T30 | GTSIL-T35 | GTSIL-T40 |
Hardness -Shore A | 04-16 | 08-10 | 14-16 | 18-22 | 23-27 | 28-32 | 25-27 | 36-40 |
Viscosity - Cps | 12000-16000 | 10000-14000 | 12000-16000 | 14000-18000 | 16000-20000 | 26000-32000 | 22000-35000 | 14000-18000 |
Mixing Ratio - % | 2% | 2% | 2% | 2% | 2% | 2% | 2% | 2% |
Tear Strength - KN/m2 | 12-16 | 19-23 | 15-18 | 19-23 | 23-27 | 28-30 | 23-27 | 22-25 |
Tensile Strength - Mpa | 3-5 | 4-6 | 3.5-5.5 | 4-6 | 4-6 | 5-7 | 4-6 | 4-6 |
Shrinkage - % | 0.3% | 0.3% | 0.3% | 0.3% | 0.3% | 0.3% | 0.3% | 0.3% |
Elongation - % | 420-530% | 400-500% | 450-550% | 450-550% | 450-550% | 350-500% | 350-500% | 350-500% |
1. Put the prototype into the container
2. Mix the liquid silicone A and B
3. Put the liquid silicone rubber into the vacuum machine for deairring.
4. Put the mix liquid silicone into the container
5. Demoulding after it is cured. Start to use the rubber molds after 24 hours.